Industry news

What are the harmful effects of over-grinding in a ball mill?

The Dangers of Over-grinding

Sliming: Gangue minerals are ground into ultra-fine "slimes," which increase pulp viscosity and impair the selectivity of the flotation process.

Over-pulverization: Valuable minerals are ground too finely, making them difficult to recover through conventional separation methods and resulting in metal loss.

Energy Waste: Grinding is the most energy-intensive operation in a mineral processing plant; over-grinding directly drives up electricity consumption.

Increased Reagent Consumption: Fine slimes have a large specific surface area, leading to higher reagent adsorption and increased reagent costs.

Dewatering Difficulties: Fine slimes reduce the efficiency of thickening and filtration, resulting in higher moisture content in the final concentrate.

These issues are precisely what staged grinding and coarse-grinding/tailings-rejection strategies aim to address. By ensuring that material is ground only to the necessary degree of fineness—applying finer grinding only where liberation is truly required—inefficient grinding can be avoided.

In terms of energy, grinding typically accounts for more than half of a plant's total electricity consumption. For every 10-percentage-point increase in fineness, the hourly throughput capacity of a mill often drops by 20% to 30%, while specific energy consumption rises—a cost that is frequently underestimated when comparing different process flowsheets.

球磨机13.jpg

How to Choose the Right Approach

Conduct Fineness Tests: Determine the relationship between target fineness and recovery rates to identify the optimal "inflection point."

Analyze Mineral Dissemination (Grain Size): If minerals are coarsely disseminated and there is a high proportion of gangue, consider coarse-grinding with tailings rejection; if the dissemination is uneven, consider staged grinding.

Compare Process Flowsheets: Evaluate options such as single-stage versus staged grinding by comparing recovery rates, energy consumption, and capital investment.

Determine Tailings Rejection/Regrinding Points: Use testing to establish the appropriate particle size for tailings rejection and the required fineness for regrinding.

Integrate Classification Equipment: Staged grinding requires the use of classification equipment to control particle size at each stage.


Contact Us

Contact: XKJ GROUP

Phone: 0086 138 3714 0277

Tel: 0086 0371-65091987

E-mail: sales01@xkjgroup.com